| UNE/EN/ISO-536 | Gramaje | g/m2 | 60 | 70 | 80 | 90 | 100 | +/-4% |
| UNE/EN-20287 | Humedad | % | 7.0 | 7.0 | 7.0 | 7.0 | 7.0 | +/-1,5 |
| UNE/EN/ISO-1924/2 | Alargamiento SM | % | 6.5 | 6.5 | 6.5 | 6.5 | 6.5 | -10% |
| UNE/EN/ISO-1924/2 | Alargamiento ST | % | 9.0 | 9.0 | 9.0 | 9.0 | 9.0 | -10% |
| UNE/EN/ISO-1924/2 | Long.Rotura SM | m | 5.500 | 5.500 | 5.500 | 5.500 | 5.000 | -10% |
| UNE/EN/ISO-1924/2 | Long.Rotura ST | m | 4.500 | 4.500 | 4.500 | 4.500 | 4.500 | -10% |
| UNE/EN/ISO-1924/2 | TEA SM | J/g | 2.1 | 2.1 | 2.1 | 2.1 | 2.1 | -10% |
| UNE/EN/ISO-1924/2 | TEA ST | J/g | 2.6 | 2.6 | 2.6 | 2.6 | 2.6 | -10% |
| UNE/EN-21974 | Ind.Rasgado SM | mN m2/g | 12.5 | 12.5 | 12.5 | 12.5 | 12.5 | -10% |
| UNE/EN-21974 | Ind.Rasgado ST | mN m2/g | 12.5 | 12.5 | 12.5 | 12.5 | 12.5 | -10% |
| UNE/EN/ISO-2758 | Indice MULLEN | (kPa m2/g)*10 | 47 | 47 | 47 | 47 | 47 | Indicativo |
| UNE/EN-20535 | Cobb 60 C | g/m2 | 25 | 25 | 25 | 25 | 25 | Max40 |
| UNE/EN-20535 | Cobb 60 T | g/m2 | 25 | 25 | 25 | 25 | 25 | Max40 |
| UNE-57066/3 | Gurley | s | 16 | 18 | 20 | 22 | 25 | +10% |
| T815om-01 | Deslizamiento | º | 18 | 18 | 18 | 18 | 18 | -10% |
| UNE/EN-20187 | ACONDICIONAMIENTO DE MUESTRAS | |||
| Humedad relativa | % | 50.0 | +/-2% | |
| Temperatura | ºC | 23.0 | +/-1ºC | |